It's just a steel post, not fancy or artistic and doesn't stand out, but it serves a very important roll in the Agriculture world.
the Galvanized T-Post function is extremely valuable when used with wire or mesh in keeping livestock, horses, from leaving a pasture.
We see them on almost every farm or ranch. It's just a simple steel post, however it's function is extremely valuable when used with wire or mesh in keeping livestock, horses, from leaving a pasture. It can be used to keep deer or other wildlife from entering a farmers field of crops.
Made from re-rolling High Carbon 100 % recycled Rail Steel, the T-Post is extremely strong with a average tensile strength of 128,000 pounds and a average yield of 78,000 pounds. T-Post can be painted or Galvanized, depending on the environment the T-Post will be exposed to. The Galvanized T-Post provides the extra protection where a farm or ranch is exposed to salt air, heavy containment of livestock, or just to add years of life to the T-Post.
With a variety of lengths available, the T-Post provides unmatched durability, strength and years of protection to farms and ranches.
Newly Complete
Food & Agriculture
Other/Unsure
Rural
South Central Texas, TX United States
Coating Durability, Corrosion Performance, Life-Cycle Cost, Prior HDG Experience, Quality of HDG, Sustainability
Entire surface area of T-post
Steel: 23
HDG: 23