Allmand Emergency Lighting Towers
Used extensively in construction sites and emergency situations, the Allmand Emergency Lighting Towers give light to numerous projects. Project lighting must be reliable because it keeps those under its spotlight protected. In construction, the light light towers prevent accidents. In emergency situations, they help guide people to safety. These applications require the lighting equipment to be sturdy and accountable. The assembly was hot dip-galvanized (HDG) to keep the lighting unit reliable and protected from corrosion. Any weakness in the lighting tower could lead to potential harm to those whom it is watching over.
HDG provides double corrosion protection; both cathodic (sacrificial) and barrier. The cathodic protection refers to the zinc coating’s ability to absorb the corrosive environment so the steel structure underneath is protected. The zinc coating is also a protective barrier between the steel and outside elements. With both types of protection, the Allmand lighting towers will bring focus to a century of projects and emergency situations.