Is hot-dip galvanized steel considered anti-sparking?
Yes, hot-dip galvanized coatings are anti-sparking and nonincendiary as are most zinc coatings. The exception is zinc coating alloys that have 30 to 55% aluminum. It is
What welding material yields normal zinc coatings?
For stick rod application, Lincoln Electric’s Fleetweld 35 LS (AWS E 6011) seems to work quite well to produce a galvanized coating thickness closest to the
Practices to avoid warpage and distortion of hot-dip galvanized articles
ASTM A384 Standard Practice for Safeguarding Against Warpage and Distortion During Hot-Dip Galvanizing of Steel Assemblies identifies factors and types of assemblies and weldments prone