Inspection of Hot-Dip Galvanized Steel

This course is intended to train individuals on the proper inspection techniques and requirements for hot-dip galvanized steel products. There are four sections in this course:

  • Hot-Dip Galvanizing Process
  • Galvanizing Standards
  • Types of Inspection
  • Repair

Upon completion of this course, you should be able to recognize specification requirements and perform all inspection steps to ensure conformance with the requirements. Additionally, any inspector who completes the course, and passes the test (80% or better) will receive a printable Certificate of Completion and will be listed on the AGA website as an inspector.

Disclaimer

The information contained in this course has been compiled by the American Galvanizers Association (AGA), a not-for-profit trade association whose members represent the after-fabrication hot-dip galvanizing industry throughout the United States, Canada, and Mexico. The AGA makes no endorsement and offers no evaluation of any vendor’s products, whether listed here or not.